329
Table 11 Selective oxidation of HMF to FDCA using Ru-supported catalysts
Entry Catalyst
Solvent
T(°C)/t(h)
HMF conv.
(%)
FDCA yield
(%)
References
1
Ru(OH)x/CeO 2 H 2 O
140/20/18 –
60
[164]
2
Ru/C
H 2 O
140/1
99.9
23.7
[165]
3
Ru/γ-Al 2 O 3
H 2 O
140/1
32.4
0
4
Pd/C
H 2 O
140/1
35.1
0
5
Pt/C
H 2 O
140/1
100
56.3
6
Ru/CTF
H 2 O
140/1
100
41.4
7
Ru/CTF
H 2 O
140/3
100
77
8
Ru/C + NaOH
H 2 O
120/5
100
69
[166]
9
Ru/C + K 2 CO 3
H 2 O
120/5
100
80
10
Ru/C + Na 2 CO 3 H 2 O
120/5
100
93
11
Ru/C + HT
H 2 O
120/5
100
90
12
Ru/C + CaCO 3 H 2 O
120/5
100
95
13
Ru/C
H 2 O
120/10
100
88
14
Ru/MnCo 2 O 4
H 2 O
120/10
100
99.1
[167]
15
Ru/CoMn 2 O 4
H 2 O
120/10
100
82.2
16
Ru/MnCo 2 CO 3 H 2 O
120/10
99.9
69.9
17
Ru/MnO 2
H 2 O
120/10
98.8
31.1
18
Ru/CoO
H 2 O
120/10
91.1
17.8
19
ZrP-Ru
H 2 O
110/12
14
11
[168]
20
ZrP-Ru
MeCN
110/12
19
20
21
ZrP-Ru
Ethanol
110/12
20
4
a
22
ZrP-Ru
DMSO
110/12
39
27
a
23
ZrP-Ru
MIBK
110/12
55
19
a
24
ZrP-Ru
Toluene
110/12
91
26
a
25
ZrP-Ru
p-Cl
toluene
110/12
95
28
a
26
ZrP-Ru + K 2 CO 3 p-Cl
toluene
150/6
100
34
a
27
Ru/ZrO 2 H -SBA H 2 O
120/16
97
87
a
[169]
28
Ru/ZrO 2 H -aero H 2 O
120/16
100
97
a
29
Ru/MgAlO
H 2 O
140/4
100
99
[170]
30
Ru/MgO
H 2 O
140/4
80
58
31
Ru/La 2 O 3
H 2 O
140/4
4.6
0.8
32
Ru/CeO 2
H 2 O
140/4
89
7.0
33
Ru/ZrO 2
H 2 O
140/4
100
0
34
Ru/HAP
H 2 O
120/1
100
>99
[171]
35
Pt/CNT
H 2 O
100/12
100
98
[172]
36
Pd/CNT
H 2 O
100/12
100
96
37
Ru/CNT
H 2 O
100/12
100
93
38
Co/CNT
H 2 O
100/12
97
96
b
39
Ni/CNT
H 2 O
100/12
97
92
b
(continued)
Levulinic Acid- and Furan-Based Multifunctional Materials: Opportunities…