Fig. 15.4 SEM micrograph and (a–c) EDS maps of the 70% B 6 O + 30% B 4 C composite. The lighter regions in the matrix phase (top left) are due
to a higher volume fraction of porosity and correlate with a high oxygen signal, indicative of a higher amount of B 6 O
Fig. 15.3 (a) SEM micrograph and (b–d) EDS maps of the monolithic B 6 O sample