7.4 Molten Salt-Assisted Conversion of PET into Carbon …
121
Fig. 7.7 (Upper panel) XRD and (down panel) Raman spectra of the carbon material obtained by
heating the mixture of PET and NaCl to 1100 °C and 1300 °C, followed by cooling and washing
process, reproduced from Ref. [24], copyright 2019, with permission from Elsevier