329
Fig. 8 Variation of % CH 4 conversion for (2.6, 5.0 and 7.5) ODRM during 4 h TOS over 10% Ni/
MgAl 2 O 4 catalyst at 600 °C
Fig. 9 Variation of % CH 4 conversion for (2.6, 5.0 and 7.5) ODRM during 4 h TOS over 10% Ni/
MgAl 2 O 4 catalyst at 750 °C
Flue Gas Treatment via Dry Reforming of Methane