632
C. Wang et al.
of sulfuric acid. Considering the comprehensive results, the flotation index of new
scheme is as good as that of HAPP.
Conclusions
In this research, an environment friendly and cost-effective approach was developed
for the beneficiation of high sulfur lead–zinc sulfide ore from Fankou mine, Guangdong Province, China. The closed circuit flotation generates concentrates with Pb
grade of 60.84%, recovery of 82.60% and Zn grade of 56.22%, recovery of 95.26%,
S grade of 46.78, recovery of 64.47 by new method. Both the reagents’ costs and
power requirements were minimized, resulting in 4.5 million RMB annual savings
for the Fankou mine.
Précédent

- 609/937